Graphitized Multi Walled Carbon Nanotubes

Graphititzed Multi Walled Carbon Nanotubes

Graphitized Multi Walled Carbon Nanotubes are made from our standard MWNTs products.

They are graphitized by annealing under inert gas for ~20 hours at 2800°C. The thermal treatment produces multi-walled carbon nanotubes with the highest graphite crystallization,  electrical conductivity, and the best oxidization resistance.

The electrical conductivity can be compared with graphite powder, and the ignition temperature can reach 800°C.

To find the price for a specific product and quantity, please click thru to the individual product page and enter the quantity you need. Our website will display the price for that specific quantity.

Quotes are available online thru our cart. Simply add the products and quantities you need into the cart and then you can print or download a quote.

Showing 1–12 of 18 results

  • COOH Functionalized Graphitized Multi Walled Carbon Nanotubes 10-20nm

    COOH Functionalized Graphitized Multi Walled Carbon Nanotubes 10-20nm

    $2.80 - $35.00 / per gram
    Select options
  • TEM image of COOH Functionalized Graphitized Multi Walled Carbon Nanotubes 20-30nm

    COOH Functionalized Graphitized Multi Walled Carbon Nanotubes 20-30nm

    $3.50 - $30.00 / per gram
    Select options
  • Graphitized Multi Walled Nanotubes 30-50nm

    COOH Functionalized Graphitized Multi Walled Carbon Nanotubes 30-50nm

    $3.49 - $25.00 / per gram
    Select options
  • COOH Functionalized Graphitized Multi Walled Carbon Nanotubes 50nm

    COOH Functionalized Graphitized Multi Walled Carbon Nanotubes 50nm

    $2.80 - $25.00 / per gram
    Select options
  • COOH functionalized graphitized multi walled carbon nanotubes 8-15nm

    COOH Functionalized Graphitized Multi Walled Carbon Nanotubes 8-15nm

    $4.49 - $45.00 / per gram
    Select options
  • Flexiphene Aqueous Nanomaterial Emulsions

    Read more
  • Flexiphene Solvent Based Nanomaterial Emulsions

    Read more
  • Flexiphene Surfactant Solutions

    Read more
  • graphitized multi walled carbon nanotubes 10-20nm

    Graphitized Multi Walled Carbon Nanotubes 10-20nm

    $3.65 - $50.00 / per gram
    Select options
  • graphitized multi walled carbon nanotubes 20-30nm

    Graphitized Multi Walled Carbon Nanotubes 20-30nm

    $2.99 - $40.00 / per gram
    Select options
  • graphitized multi walled carbon nanotubes 50nm

    Graphitized Multi Walled Carbon Nanotubes 50nm

    $3.00 - $10.00 / per gram
    Select options
  • graphitized multi walled carbon nanotubes 8-15nm

    Graphitized Multi Walled Carbon Nanotubes 8-15nm

    $3.65 - $50.00 / per gram
    Select options

Graphitized Carbon Nanotubes Properties

GMWNTs have the highest strength, conductivity, and crystallinity. Thermal annealing increases those properties but reduces specific surface area (SSA) by 50%. GMWNTs are harder to disperse than typical MWNTs and may require higher dispersant use.

Showing 1–12 of 18 results